CONCRETE
As soon as forming and molding are removed, preparation should begin. Grinding, vacuum or abrasive blasting to a 1mm profile. Remove all laitance. Repair defects...sacking should be done to all vertical surfaces. Remove all dirt and residue by vacuum and pressure washing with white vinegar solution, air dry. Do Not use petroleum fired heaters! AQUAPLY-SLP will be the primer and top coat and can designed to utilize moisture and displace it. Please request moisture application formula. Mix equal amounts by volume, parts A and B with a mechanical mixer at slow speed until completely mixed.
DO NOT ADD THINNERS
Apply SL-P by spray, roller epoxy grade) or squeegee,
...anti-foaming and bubble breakers have been added,
however, bubbles will appear during the penetration of
the coating... it is necessary to go over the area with a spiny roller prior to additional coats. Viscosity can be
lowered by warming product.
Additional costs are applied when the prior coat is thumb print tacky. No sanding is required between coats if this procedure is followed. This allows for a wet on wet application forming an absolute bonding of coats.
EQUIPMENT
|
TROWEL AND BROADCAST
REPAIRS Repairs to damaged or chipped areas are quite
easy. Area should be segregated, cleaned and degreased.
White vinegar and water are fine. AQUAPLY SLP then applied to the segregated area. Add appropriate
fillers and colors to match.
METALS
|
| Home |
| Products |
| Applications |
| Contact Us |